CEM IV/B (P) 32.5 R CEM IV/B (P) 32.5 R
 
CEM IV/B (P) 32.5 R
Product
Pozzolanic Cement

Standard
TS EN 197-1:2002 CEM IV/B (P) 32.5 R

Product Description
The cement is produced by grinding at least one type of mineral additive (pozzolana) prescribed by standards (max. %55) with portland clinker by addition of a certain amount of retarder  (generally gypsum).

The product delivers the strength values respectively in late periods compared to CEM I and CEM II types. Water/cement ratio is respectively higher. It is much more resistant to alkali and aggregate reactions. It is best for repairing works, foundation filling and used in stucco and building chemicals manufacturing.

Physical Characteristics
Nuh Çimento StandardUnit
Solidification Start/End
190min. 75 minute
Solidification End
240-minute
Volume Expansion
1max. 10 cm
Specific Surface (Blaine)
5357-cm2/g
Liter Weight
847-g/l
2-day Resistance
14.5min. 10 MPa
28-day Resistance

35.7

min./max. 32.5/52.5 MPa


Chemical Characteristics

Nuh Çimento StandardUnit
SO3
2.74max. 3.5 %
Cl-
0.01>max. 0.1 %
Pozzuolana Test
Positivesatisfies the test

Packaging Type
Sold in bulk or in 25-50 kg. kraft bags.

Quality Control
Our product is certified by Council for Quality and Environment (K.Ç.K.) according to TS EN 197-1:2002 to use CE marking in Europe.

For Information
Beyhan Üçyigit, Quality Control Vice Manager, Extension: 2050-2051
Abdülhamit Akçay, Export Chief, Extension: 2075

update
This page was updated on 10/08/2010 and includes the packaging analysis results from 01-30/06/2010